Drawing dies are consumables. How we maintain them decides three things: surface quality on the wire, drawing energy per tonne, and yield. We inspect and rotate dies on a fixed schedule and pull one out of service the moment its wear…
Annealed wire that arrives soft, clean and ready to form
Our annealed wire line runs in 2020 on inter-annealed and full-annealed cycles depending on the customer’s tensile target. Coating-ready surface is standard. Because we anneal in-house, we can respond quickly when a customer says “same grade, softer, ship this week.” That…
Annealing furnace — protective atmosphere and the surface it delivers
Our annealing furnace runs on a protective atmosphere for controlled surface finish. Full anneal or inter-anneal cycles are chosen by the target tensile and by what the customer intends to do next. Full anneal delivers the softest wire; inter-anneal preserves more…
Cold-drawn Ø1.00 – Ø14.00 mm — our workhorse family
Cold-drawn wire remains the backbone of what leaves our Muradiye OSB plant in 2019. We draw Ø1.00 to Ø14.00 mm from low-carbon SAE 1006/1008/1010 wire rod, in bright or super-bright finish. Tensile strength typically lands between 500 and 1050 N/mm² depending…
Wire rod incoming inspection — the earliest quality decision we make
Every coil of wire rod that arrives at Muradiye OSB gets inspected before it enters our drawing bays. We check the mill certificate, cross-check hardness ourselves, and log any surface finding. It sounds obvious. But the earlier you catch a rod-quality…
Cut-to-length wire and why the length tolerance matters
Cut-to-length wire looks like a commodity from the outside. Inside a fastener mill or a welding-electrode plant, one millimetre of length variance across a pallet is a real problem. In 2018 we run straightening and cutting lines that hold length tolerance…
Tensile scatter within a coil — the number that matters most
Tensile scatter within a single coil is the technical variable that most affects downstream customers. A coil where every metre reads within a narrow tensile band lets a header or a bender run without adjustments; a coil with wide scatter forces…
Annealed wire that arrives soft, clean and ready to form
Our annealed wire line runs in 2017 on inter-annealed and full-annealed cycles depending on the customer’s tensile target. Coating-ready surface is standard. Because we anneal in-house, we can respond quickly when a customer says “same grade, softer, ship this week.” That…
Drawing die maintenance — small things that decide our tonne cost
Drawing dies are consumables. How we maintain them decides three things: surface quality on the wire, drawing energy per tonne, and yield. We inspect and rotate dies on a fixed schedule and pull one out of service the moment its wear…
Cold-drawn Ø1.00 – Ø14.00 mm — our workhorse family
Cold-drawn wire remains the backbone of what leaves our Muradiye OSB plant in 2016. We draw Ø1.00 to Ø14.00 mm from low-carbon SAE 1006/1008/1010 wire rod, in bright or super-bright finish. Tensile strength typically lands between 500 and 1050 N/mm² depending…